Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 275000 - 950000 cP | 275000 - 950000 cP | Thixotropic |
ND Industries 732 Gasket Maker Flexible Flexible Parts. General Purpose |
|||
Viscosity | 12.0 - 950000 cP | 12.0 - 950000 cP | Average value: 118000 cP Grade Count:64 |
Overview of materials for Methacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Viscosity | 275000 - 950000 cP | 275000 - 950000 cP | Thixotropic |
Loctite® Gasket Eliminator® 515 Flange Sealant Anaerobic GasketingLoctite® 515 Flexible Cure Gasket Eliminator® Flange SealantMakes flexible gaskets for rigid machined flanges with less than 0.050" gap. Flexes with flanges that move in servic.. |