Physical Properties Metric English Comments
Viscosity 112 - 127 cP
112 - 127 cP
ASTM D445
ExxonMobil Jayflex™ DIDP (0.2% BPA) Plasticizer (European Grade)
Availability: Europe, Middle East & AfricaInformation provided by ExxonMobil