Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 1050 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1000 - 1050 cP

@Temperature 35.0 °C
1000 - 1050 cP

@Temperature 95.0 °F
Dynamic viscosity
C.O.I.M. PLAXTER® P 42 Polymeric Plasticizer
Description: Formulated with PVC, it is used in the field of adhesive tapes.Information provided by P.A.T. Products, Inc.
Copyright © lookpolymers.com All Rights Reserved