Polymer Property : Viscosity = 10.5 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 10.5 - 18 cP
10.5 - 18 cP
Abatron Primkote G A/B Waterborne Epoxy Primer/Sealer for Green Concrete
Primkote G is a waterborne epoxy system for priming and sealing floors. It contains a gray resin compound (Part A) and a clear hardener (Part B). It conditions concrete and other substrates for epox..