Physical Properties Metric English Comments
Viscosity 1.40e+7 cP

@Shear Rate 120 1/s,
Temperature 230 °C
1.40e+7 cP

@Shear Rate 120 1/s,
Temperature 446 °F
Noltex Soarnol® DC3203F Ethylene Vinyl Alcohol Copolymer
Low ethylene content. Suitable for use in packaging material used at normal temperature and humidity. Ethylene content 32 mol%. Volatile matter 0.3%.Information provided by Soarus, LLC. In the Un..