Physical Properties Metric English Comments
Viscosity 0.90 cP
0.90 cP
Inherent; ASTM D1243
Formosa Plastics Formolon® 24A PVC
PVC Homopolymer Dispersion Resin F-24A is a low molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compounds as well as other applica..
Viscosity 0.90 cP
0.90 cP
Inherent; ASTM D5225
Formosa Plastics Formolon® 622E PVC
Rigid Extrusion Resin F622E is a medium-low molecular weight PVC designed primarily for rigid extrusion applications. This product has excellent dry flow characteristics, making it desirable for dry..
Viscosity 0.90 cP
0.90 cP
Inherent; ASTM D5225
Formosa Plastics Formolon® 622S PVC
Homopolymer Siding Grade Resin F622S is a medium-low molecular weight PVC homopolymer designed primarily for rigid extrusion applications, but it is also suitable for many flexible applications. Thi..