Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.85 cP | 0.85 cP | Inherent; ASTM D1243 |
Formosa Plastics Formolon® 265 PVC PVC Copolymer Blending Resin F-265 is a fine particle size polyvinyl chloride vinyl acetate copolymer plastisol blending resin. The product has been designed for use in application where rapid gelat.. |