Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.60 cP @Temperature 25.0 °C |
0.60 cP @Temperature 77.0 °F |
|
Permabond POP Polyolefin Primer Permabond® Polyolefin Primer has been developed for surface treatment of polyolefins, PTFE and silicones prior to bonding with Permabond® Cyanoacrylate adhesives. Due to their low surface energy, .. |
|||
Viscosity | 0.60 cP @Temperature 25.0 °C |
0.60 cP @Temperature 77.0 °F |
|
Asahi Glass ASAHIKLIN AK-225DH Hydrochlorofluorocarbon Solvent AK-225DH was developed as a solvent dewatering and drying system to remove water from the surface of various parts and assemblies. AK-225DH is a mixture of AK-225 and a drying agent to give it rapid.. |
|||
Viscosity | 0.60 cP @Temperature 25.0 °C |
0.60 cP @Temperature 77.0 °F |
|
Asahi Glass ASAHIKLIN AK-225G Hydrochlorofluorocarbon Solvent AK-225G is an environmentally sensible HCFC. It is thermally stable, nonflammable and recoverable by distillation with no decomposition. It has substantially lower global warming potential (GWP) th.. |