Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.50 cP @Temperature 25.0 °C |
0.50 cP @Temperature 77.0 °F |
|
LyondellBasell THF Tetrahydrofuran Information provided by Lyondell. |
|||
Viscosity | 0.50 cP @Temperature 200 °C |
0.50 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3320 Polyester, Flake Low molecular weight type UE3200, High OH type, Resin modifier, Resin raw materialUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their application.. |
|||
Viscosity | 0.50 cP | 0.50 cP | dynamic |
Dow Corning OS-10 Information provided by Dow Corning |