Material Notes:
Information provided by Lyondell.
Physical Properties Metric English Comments
Specific Gravity 0.886 g/cc
0.886 g/cc
20/20°C
Density 0.888 g/cc

@Temperature 20.0 °C
0.0321 lb/in³

@Temperature 68.0 °F
Solubility in Water 100 %
100 %
20°C
Viscosity 0.50 cP

@Temperature 25.0 °C
0.50 cP

@Temperature 77.0 °F
Molecular Weight 72 g/mol
72 g/mol
Vapor Pressure 0.172 bar

@Temperature 20.0 °C
129 torr

@Temperature 68.0 °F
Evaporation Loss 8.0 %
8.0 %
n-BuAc=100%
Surface Tension 26 dynes/cm
26 dynes/cm
25°C
Thermal Properties Metric English Comments
Boiling Point 66.0 °C
151 °F
at 760 mmHg
Flash Point -14.0 °C
6.80 °F
Tag Closed Cup
Optical Properties Metric English Comments
Refractive Index 1.407

@Temperature 25.0 °C
1.407

@Temperature 77.0 °F