Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.49 cP @Temperature 25.0 °C |
0.49 cP @Temperature 77.0 °F |
|
Enviro Tech International EnSolv® n-Propyl Bromide Vapor Degreasing Solvent EnSolv is the perfect direct replacement for TCE, Perchloroethylene, 1,1,1-Trichloroethane and other hazardous vapor degreasing and general use solvents for critical applications such as oxygen serv.. |
|||
Viscosity | 0.49 cP | 0.49 cP | [mPa.s] |
BASF Methyl Acrylate Formula: C4H6O2CAS: 96-33-3Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: Methyl acrylate forms homopolymers and copolymers. Copolymer.. |