BASF Methyl Acrylate

Category Fluid
Manufacturer BASF
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Methyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formula: C4H6O2CAS: 96-33-3Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: Methyl acrylate forms homopolymers and copolymers. Copolymers of methyl acrylate can be prepared with acrylic acid and its salts, amides and esters, and with methacrylates, acrylonitrile, maleic acid esters, vinyl acetate, vinyl chloride, vinylidene chloride, styrene, butadiene, unsaturated polyesters and drying oils, etc. Methyl acrylate is also a very useful feedstock for chemical syntheses, because it readily undergoes addition reactions with a wide variety of organic and inorganic compoundsInformation provided by BASF
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
Viscosity 0.49 cP
0.49 cP
[mPa.s]
Molecular Weight 86 g/mol
86 g/mol
Vapor Pressure 0.00905 bar
6.79 torr
Thermal Properties Metric English Comments
Specific Heat Capacity 2.00 J/g-°C
0.478 BTU/lb-°F
of Liquid
Melting Point -75.0 °C
-103 °F
Freezing Point
Boiling Point 80.0 °C
176 °F
Optical Properties Metric English Comments
Refractive Index 1.404
1.404
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
ASTM E203
Descriptive Properties Value Comments
Assay >99.8%
Color <10
APHA, ASTM D1209
Heat of Polymerization 950 kJ/kg
Latent Heat of Evaporation at Boiling Point 385.1 kJ/kg