Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 7.5 g/10 min @Load 5.00 kg, Temperature 240 °C |
7.5 g/10 min @Load 11.0 lb, Temperature 464 °F |
ISO 1133 |
Polykemi AB SCANLON A 5005 PA/ABS-Blend Information provided by Polykemi AB |
|||
Melt Index of Compound | 7.5 g/10 min @Load 5.00 kg, Temperature 240 °C |
7.5 g/10 min @Load 11.0 lb, Temperature 464 °F |
ISO 1133 |
Polykemi AB SCANLON A 5005B PA/ABS-Blend Information provided by Polykemi AB |
|||
Melt Index of Compound | 7.5 g/10 min @Load 5.00 kg, Temperature 240 °C |
7.5 g/10 min @Load 11.0 lb, Temperature 464 °F |
ISO 1133 |
Polykemi AB SCANLON A 5005B UV PA/ABS-Blend Information provided by Polykemi AB |
|||
Melt Index of Compound | 7.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
7.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238G |
Total Finaclear® 520 Clear Impact Polystyrene
(discontinued **) Finaclear® 520 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles. Complemented by inherent repr.. |
|||
Melt Index of Compound | 7.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
7.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238G |
Total Finaclear® 521 Clear Impact Polystyrene
(discontinued **) Finaclear® 521 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with othe.. |
|||
Melt Index of Compound | 7.5 g/10 min | 7.5 g/10 min | ASTM D1238 |
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin AFFINITY™ PT 1450G1 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. The resin is for monolayer and co-extrusion coating that offers excellent low temperature seal initiation, ult.. |
|||
Melt Index of Compound | 7.5 g/10 min @Load 5.00 kg, Temperature 372 °C |
7.5 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
3M Dyneon™ FEP 6307 R2RZ Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6307 R2RZ is a special version of Dyneon FEP 6307 wire jacketing grade FEP with an added nucleating agent for improved foaming in gas injection extrusion processes. As the gas expands and.. |