Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Index of Compound = 6.2 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 3.5 - 6.2 g/10 min
3.5 - 6.2 g/10 min
II Preparation
Sibur ABS 1106M Extrusion Grade ABS Plastic
With high thermal and light resistance for production of sheets with following pneumatic and vacuum formation of internal parts for refrigerators and other articles of technical purpose.
Copyright © lookpolymers.com All Rights Reserved