Material Notes:
With high thermal and light resistance for production of sheets with following pneumatic and vacuum formation of internal parts for refrigerators and other articles of technical purpose.
Physical Properties Metric English Comments
Water Absorption <= 0.30 %
<= 0.30 %
Melt Index of Compound 1.0 - 3.5 g/10 min
1.0 - 3.5 g/10 min
I Preparation
3.5 - 6.2 g/10 min
3.5 - 6.2 g/10 min
II Preparation
Mechanical Properties Metric English Comments
Elongation at Break >= 25 %
>= 25 %
Izod Impact, Notched (ISO) >= 19.6 kJ/m²
>= 9.33 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point <= 95.0 °C
<= 203 °F
Optical Properties Metric English Comments
Gloss 50 %
50 %
Chemical Properties Metric English Comments
Styrene Content <= 0.050 %
<= 0.050 %
Descriptive Properties Value Comments
Acrylonitrile Content <.001
Impact Tension Strength >19.6 MPa
Users viewing this material also viewed the following: