Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 39 g/10 min @Load 10.0 kg, Temperature 220 °C |
39 g/10 min @Load 22.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycolac® MG94 ABS (Europe-Africa-Middle East) Superior flow, injection molding ABS. Good impact. For thin-wall applications. |