Polymer Property : Melt Index of Compound = 34 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 34 g/10 min

@Load 2.16 kg,
Temperature 265 °C
34 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® EH7025AG PBT+PET
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
Melt Index of Compound 34 g/10 min

@Load 2.16 kg,
Temperature 265 °C
34 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
Melt Index of Compound 34 g/10 min

@Load 2.16 kg,
Temperature 265 °C
34 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
Melt Index of Compound 34 g/10 min

@Load 2.16 kg,
Temperature 250 °C
34 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
Melt Index of Compound 34 g/10 min

@Load 2.16 kg,
Temperature 250 °C
34 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
Melt Index of Compound 34 g/10 min

@Load 2.16 kg,
Temperature 250 °C
34 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® V2000DM PBT
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.