Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.0 - 3.0 g/10 min | 1.0 - 3.0 g/10 min | |
Sibur ABS 1106 Extrusion Grade ABS Plastic With high deformation properties and sanitary-hygienic properties for production of sheets with following pneumatic and vacuum forming of internal parts of refrigerators, as well as for compounding .. |
|||
Melt Index of Compound | 2.0 - 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.0 - 3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTRYL® 18 MA 02 Copolymer Ethylene - Methyl Acrylate LOTRYL® 18 MA 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 18 MA 02 is a polymer of .. |
|||
Melt Index of Compound | 2.0 - 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.0 - 3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTRYL® 14 MGC 02 Copolymer Ethylene - Methyl Acrylate LOTRYL® 14 MGC 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the Methyl Acrylate content, LOTRYL® 14 MGC 02 is a polymer o.. |