Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 2.1 g/10 min | 2.1 g/10 min | cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro.. |
|||
Melt Index of Compound | 2.1 g/10 min | 2.1 g/10 min | cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® 127UVE RD402 Acetal Homopolymer
(Unverified Data**) Delrin® 127UVE RD402 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro.. |
|||
Melt Index of Compound | 2.1 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.1 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Lendell Parapet HH-1000L PMMA, Heat Resistant |
|||
Melt Index of Compound | 2.1 - 3.9 g/10 min | 2.1 - 3.9 g/10 min | ASTM D1238-82 |
DuPont Elvax® 40L-03 Ethylene-Vinyl Acetate Copolymer Resin Elvax® 40L-03 is an ethylene-vinyl acetate copolymer that is useful in many wire and cable applications because of its excellent mechanical, thermal, and low-smoke properties. The melt index is ap.. |
|||
Melt Index of Compound | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
Chevron Phillips MarFlex® 1125 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for blown film applications that require: Good impactNo slip, includes antiblockGood processabilityGood sealabilityGood drawdown Applications: Typi.. |
|||
Melt Index of Compound | 2.1 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow 560.00 Developmental Performance Polypropylene Polymer OverviewConsistent processabilityExcellent gloss before and after thermoformingUV stabilized for increased weatherabilityD 560.00 Performance Polymer is designed as a co-extrusion cap layer for extr.. |
|||
Melt Index of Compound | 2.1 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow 560.01 Developmental Performance Polypropylene Polymer OverviewConsistent processabilityHigh glossGood regrind stabilityContains U.V. stabilizers for increased weatherabilityD 560.01 Performance Polymer is intended for use in extrusion blow molding, she.. |
|||
Melt Index of Compound | 2.1 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem INSPIRE™ 117 Performance Polypropylene Polymer D 117.00 Developmental Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistanc.. |