Dow 560.00 Developmental Performance Polypropylene Polymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow 560.00 Developmental Performance Polypropylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OverviewConsistent processabilityExcellent gloss before and after thermoformingUV stabilized for increased weatherabilityD 560.00 Performance Polymer is designed as a co-extrusion cap layer for extrusion grade TPOs where high gloss and weatherability is desired.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 2.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus, 1% Secant 1070 MPa
155000 psi
ASTM D790A
Izod Impact, Notched 2.94 J/cm
5.51 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.1 °C
187 °F
Unannealed; ASTM D648