Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 6.0 - 11 g/10 min | 6.0 - 11 g/10 min | |
Sibur 21080 1st Grade Polypropylene for Production of Syringe For production of syringe and products of complicated profile for technical and domestic purpose. |
|||
Melt Index of Compound | 6.0 - 11 g/10 min | 6.0 - 11 g/10 min | |
Sibur 21080 Superior Quality Polypropylene for Production of Syringe For production of syringe and products of complicated profile for technical and domestic purpose. |
|||
Melt Index of Compound | 6.0 - 11 g/10 min @Load 12.0 kg, Temperature 220 °C |
6.0 - 11 g/10 min @Load 26.5 lb, Temperature 428 °F |
ASTM D1238, ISO 1133 |
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene |