Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.23 - 0.30 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.23 - 0.30 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc.. |
|||
Melt Index of Compound | 0.23 - 0.30 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.23 - 0.30 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding.. |
|||
Melt Index of Compound | 0.23 - 0.30 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.23 - 0.30 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product.. |
|||
Melt Index of Compound | 0.23 - 0.30 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.23 - 0.30 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,.. |