Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Index of Compound = 0.23 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 0.23 - 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.23 - 0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film
The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc..
Melt Index of Compound 0.23 - 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.23 - 0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film
The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding..
Melt Index of Compound 0.23 - 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.23 - 0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film
The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product..
Melt Index of Compound 0.23 - 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.23 - 0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade
The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,..