Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0070 cm/cm @Thickness 1.60 mm |
0.0070 in/in @Thickness 0.0630 in |
Transverse; DAM |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm @Thickness 6.35 mm |
0.0070 - 0.0090 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® M-1812 Polypropylene Homopolymer, 45% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0070 cm/cm @Thickness 3.17 mm |
0.0070 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0070 - 0.013 cm/cm @Thickness 1.60 mm |
0.0070 - 0.013 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 4140-201D 40% Glass Fiber Filled Product Description: A glass fiber 40% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0070 - 0.011 cm/cm @Thickness 3.00 mm |
0.0070 - 0.011 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-400G15 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm @Thickness 1.00 mm |
0.0070 - 0.010 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm @Thickness 1.00 mm |
0.0070 - 0.010 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm @Temperature 105 °C |
0.0070 in/in @Temperature 221 °F |
ASTM D3392 |
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm @Temperature 105 °C |
0.0070 in/in @Temperature 221 °F |
ASTM D3392 |
DuPont™ Nomex® Type 993, 60 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm @Temperature 105 °C |
0.0070 in/in @Temperature 221 °F |
ASTM D3392 |
DuPont™ Nomex® Type 993, 80 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm @Thickness 3.20 mm |
0.0070 in/in @Thickness 0.126 in |
Transverse; ASTM D955 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.0070 - 0.011 cm/cm @Thickness 1.60 mm |
0.0070 - 0.011 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP PBT 3010-104 10% Glass Fiber Filled Product Description: PBT glass fiber 10% reinforced injection molding grade.Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent.. |
|||
Linear Mold Shrinkage | 0.0070 cm/cm @Thickness 3.20 mm |
0.0070 in/in @Thickness 0.126 in |
Transverse |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |