Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.69 g/cc @Temperature 110 °C, Time 86400 sec |
0.0972 lb/in³ @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories A65 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.69 g/cc @Temperature 1500 °C, Time 10800 sec |
0.0972 lb/in³ @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories M55 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.69 g/cc @Temperature 1500 °C, Time 10800 sec |
0.0972 lb/in³ @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories SW83 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.69 g/cc @Temperature 1500 °C, Time 10800 sec |
0.0972 lb/in³ @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories SW87 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |