Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.66 g/cc

@Temperature 1000 °C,
Time 10800 sec
0.0961 lb/in³

@Temperature 1830 °F,
Time 3.00 hour
2.66 g/cc

@Temperature 1500 °C,
Time 10800 sec
0.0961 lb/in³

@Temperature 2730 °F,
Time 3.00 hour
2.69 g/cc

@Temperature 110 °C,
Time 86400 sec
0.0972 lb/in³

@Temperature 230 °F,
Time 24.0 hour
Porosity 19.5 %

@Temperature 110 °C,
Time 86400 sec
19.5 %

@Temperature 230 °F,
Time 24.0 hour
24 %

@Temperature 1500 °C,
Time 10800 sec
24 %

@Temperature 2730 °F,
Time 3.00 hour
24.5 %

@Temperature 1000 °C,
Time 10800 sec
24.5 %

@Temperature 1830 °F,
Time 3.00 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0034335 GPa

@Temperature 110 °C,
Time 86400 sec
0.49799 ksi

@Temperature 230 °F,
Time 24.0 hour
0.003924 GPa

@Temperature 1000 °C,
Time 10800 sec
0.5691 ksi

@Temperature 1830 °F,
Time 3.00 hour
0.003924 GPa

@Temperature 1500 °C,
Time 10800 sec
0.5691 ksi

@Temperature 2730 °F,
Time 3.00 hour
Thermal Properties Metric English Comments
Shrinkage -0.0600 %

@Temperature 110 °C,
Time 86400 sec
-0.0600 %

@Temperature 230 °F,
Time 24.0 hour
-0.0600 %

@Temperature 1000 °C,
Time 10800 sec
-0.0600 %

@Temperature 1830 °F,
Time 3.00 hour
0.050 %

@Temperature 1500 °C,
Time 10800 sec
0.050 %

@Temperature 2730 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 65 %
65 %
SiC 30 %
30 %
SiO2 1.0 %
1.0 %
Descriptive Properties Value Comments
Main Applications Blast furnace Main runner
Material Required for Estimating (kg/?) 2,700