Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0239 cm/cm
0.0239 in/in
STN 64 0808
Plastcom SLOVALEN PC 88 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized
FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with..