Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0129 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0129 cm/cm
0.0129 in/in
STN 64 0808
Plastcom SLOVALEN PH 51 T 15 Polypropylene Homopolymer, 15% Mineral Filled
FeaturesModified homopolymer PP for injection moulding with the content of 15% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application ..