Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0129 cm/cm | 0.0129 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 51 T 15 Polypropylene Homopolymer, 15% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 15% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application .. |