Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0112 cm/cm | 0.0112 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 GF 15 Polyamide 6, 15% Glass Fiber FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and .. |
|||
Linear Mold Shrinkage, Transverse | 0.0112 cm/cm | 0.0112 in/in | |
Plastcom SLOVAMID 6 GF 7 T 13 PA6, 7% glass fibre, 13% mineral filling FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooli.. |
|||
Linear Mold Shrinkage, Transverse | 0.0112 cm/cm | 0.0112 in/in | STN EN ISO 294-4 |
Plastcom SLOVAMID® 6 GF 25 FRC 4 PA6 reinforced with glass fiber, flame retarded PA 6 for injection molding, reinforced with 25 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability according to UL 94 3 at 1,6mm, glow wire at 960°C. Applic.. |
|||
Linear Mold Shrinkage, Transverse | 0.0112 cm/cm | 0.0112 in/in | |
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Linear Mold Shrinkage, Transverse | 0.0112 cm/cm @Thickness 2.00 mm |
0.0112 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsContains UV stabilizer and anti-static agentRecommended Applications:Electric.. |
|||
Linear Mold Shrinkage, Transverse | 0.0112 cm/cm | 0.0112 in/in | |
Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, DRY Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America.. |
|||
Linear Mold Shrinkage, Transverse | 0.0112 cm/cm | 0.0112 in/in | STN 64 0808 |
Plastcom SLOVAMID 66/6 GF 30 Polyamide 66/6, 30% Glass Fiber
(discontinued **) FeaturesChemically reinforced alloy PA 66 and PA 6 with 30% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and el.. |