Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0107 cm/cm | 0.0107 in/in | |
Plastcom SLOVAMID 66 GF 20 GF 10 PA66, 20% glass fibre, glass beads FeaturesPA 66 chemically reinforced with 20% glass fibre and with the content of 10 % glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can b.. |
|||
Linear Mold Shrinkage, Transverse | 0.0107 cm/cm | 0.0107 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 G 10 Polyamide 6, 10% Graphite FeaturesPA 6 for injection moulding with addition of 10% graphite, the PA surface rolling resistance force is significantly lowered. Used mainly in the product of crates and cases for bearings, sli.. |
|||
Linear Mold Shrinkage, Transverse | 0.0107 cm/cm | 0.0107 in/in | ISO 2577 |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Linear Mold Shrinkage, Transverse | 0.0107 - 0.0290 cm/cm | 0.0107 - 0.0290 in/in | Average value: 0.0170 cm/cm Grade Count:12 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage, Transverse | 0.0107 cm/cm | 0.0107 in/in | 60x60x2mm; ISO 294 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Linear Mold Shrinkage, Transverse | 0.0107 cm/cm | 0.0107 in/in | ISO 2577 |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |