Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0097 cm/cm | 0.0097 in/in | |
Plastcom SLOVAMID 66 GF 10 FRA 3 PA66, 10% glass fibre Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Linear Mold Shrinkage, Transverse | 0.0097 cm/cm | 0.0097 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 25 FRG 5 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemical reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal.. |
|||
Linear Mold Shrinkage, Transverse | 0.0097 cm/cm | 0.0097 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 25 FRI 3 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-h.. |
|||
Linear Mold Shrinkage, Transverse | 0.0097 cm/cm | 0.0097 in/in | |
Plastcom SLOVAMID 66 GF 25 FRI 3 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Linear Mold Shrinkage, Transverse | 0.0097 cm/cm | 0.0097 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 35 FRG 5 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemical reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal.. |
|||
Linear Mold Shrinkage, Transverse | 0.0097 cm/cm | 0.0097 in/in | 60x60x2; 290°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® AM 40 X H2.0 901510 Nylon 66, Glass Fiber/Mineral Reinforced PA 66, 40% glass fibers/mineral, injection molding, heat-aging stabilized, low tendency to warpInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0097 cm/cm | 0.0097 in/in | ISO 294 |
BASF Ultradur B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET Ultradur B 4040 G6 High Speed BK15029 is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable.. |
|||
Linear Mold Shrinkage, Transverse | 0.0097 cm/cm | 0.0097 in/in | ISO 2577 |
BASF Ultradur® S 4090 G6X High Speed 30% Glass Filled PBT Description: Low-warpage, easy-flowing injection molding grade with 30 % glass fibers for technical parts, for which dimensional stability is very important, reduction of wall thickness (eg, e/e hou.. |