Linear Mold Shrinkage, Transverse 0.0079 cm/cm
0.0079 in/in
Plastcom SLOVAMID 6 T 20 PA6, 20% mineral filling
FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased modulus in tension - strength of the material. PA matrix reduction. Application eg. for tools, fi..
Linear Mold Shrinkage, Transverse 0.0079 cm/cm
0.0079 in/in
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY
Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical ..
Linear Mold Shrinkage, Transverse 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RV00AEXP PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AEXP is a compound based on PA 66 resin containing Long Glass Fiber.
Linear Mold Shrinkage, Transverse 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RV00ASXP PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00ASXP is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized.
Linear Mold Shrinkage, Transverse 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RV00ASXS PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00ASXS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized
Linear Mold Shrinkage, Transverse 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RV00AXX9 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AXX9 is a compound based on PA 66 resin containing Long Glass Fiber.