Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00200 - 0.00640 cm/cm
0.00200 - 0.00640 in/in
Average value: 0.00570 cm/cm Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..