Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00040 - 0.00080 cm/cm

@Thickness 3.18 mm
0.00040 - 0.00080 in/in

@Thickness 0.125 in
ASTM D955
PolyOne Edgetek® SF2-40CF/000 NATURAL Polyphenylene Sulfide (PPS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..