Physical Properties Metric English Comments
Viscosity 99512 cP

@Shear Rate 5000 1/s,
Temperature 285 °C
99512 cP

@Shear Rate 5000 1/s,
Temperature 545 °F
ISO 11403-1 -2
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..