Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 500000 - 900000 cP

@Temperature 190 - 190 °C
500000 - 900000 cP

@Temperature 374 - 374 °F
Average value: 700000 cP Grade Count:3
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an..
Viscosity 500000 - 900000 cP

@Shear Rate 50.0 - 50.0 1/s
500000 - 900000 cP

@Shear Rate 50.0 - 50.0 1/s
Average value: 700000 cP Grade Count:3
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an..