Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 500000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 500000 cP

@Temperature 25.0 °C
500000 cP

@Temperature 77.0 °F
ET536B, Polyamine Hardener
Permabond ET536 Epoxy Resin
PERMABOND ET536 is a two-part, 1:1 mixable epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET536 forms tough bo..
Viscosity 500000 cP

@Temperature 25.0 °C
500000 cP

@Temperature 77.0 °F
at 2rpm vibration
Permabond HH167 Anaerobic Retainer
Permabond® HH167 is a high viscosity gap filling silver paste, which can be used for repairing metal machinery parts. It is ideal for repairing worn shafts, broken threads, damaged keyways and spli..
Viscosity 500000 cP

@Temperature 25.0 °C
500000 cP

@Temperature 77.0 °F
at 2 rpm vibration
Permabond MH196 Anaerobic Gasketmaker
Permabond® MH196 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po..
Viscosity 500000 cP

@Shear Rate 1.00 1/s,
Temperature 250 °C
500000 cP

@Shear Rate 1.00 1/s,
Temperature 482 °F
DSM Arnite® TM4 440 (PBT+PET)-MD20
20% Mineral Reinforced
Viscosity 500000 cP

@Shear Rate 1.00 1/s,
Temperature 250 °C
500000 cP

@Shear Rate 1.00 1/s,
Temperature 482 °F
DSM Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40
20% Glass Reinforced, 20% Glass Beads Reinforced
Viscosity 500000 cP

@Shear Rate 1.00 1/s,
Temperature 250 °C
500000 cP

@Shear Rate 1.00 1/s,
Temperature 482 °F
DSM Arnite® T06 202 /A PBT
Medium Viscosity, Injection Molding
Viscosity 500000 cP

@Shear Rate 1.00 1/s,
Temperature 250 °C
500000 cP

@Shear Rate 1.00 1/s,
Temperature 482 °F
DSM Arnite® TZ6 280 PBT-(GF+GB)40
20% Glass Reinforced, 20% Glass Beads Reinforced
Viscosity 500000 - 900000 cP

@Temperature 190 - 190 °C
500000 - 900000 cP

@Temperature 374 - 374 °F
Average value: 700000 cP Grade Count:3
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an..
Viscosity 500000 - 900000 cP

@Shear Rate 50.0 - 50.0 1/s
500000 - 900000 cP

@Shear Rate 50.0 - 50.0 1/s
Average value: 700000 cP Grade Count:3
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an..
Copyright © lookpolymers.com All Rights Reserved