Physical Properties Metric English Comments
Viscosity 89660 cP

@Shear Rate 5000 1/s,
Temperature 250 °C
89660 cP

@Shear Rate 5000 1/s,
Temperature 482 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..