Polymer Property : Viscosity = 86460 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 86460 cP

@Shear Rate 500 1/s,
Temperature 295 °C
86460 cP

@Shear Rate 500 1/s,
Temperature 563 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi..