Polymer Property : Viscosity = 856000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 856000 cP

@Shear Rate 500 1/s,
Temperature 205 °C
856000 cP

@Shear Rate 500 1/s,
Temperature 401 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)  (Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part..