Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 81000 cP @Shear Rate 5000 1/s, Temperature 215 °C |
81000 cP @Shear Rate 5000 1/s, Temperature 419 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Viscosity | 81000 cP @Shear Rate 5000 1/s, Temperature 215 °C |
81000 cP @Shear Rate 5000 1/s, Temperature 419 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Viscosity | 81000 cP @Shear Rate 5000 1/s, Temperature 235 °C |
81000 cP @Shear Rate 5000 1/s, Temperature 455 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |