Polymer Property : Viscosity = 800000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 800000 - 800000 cP

@Temperature 320 - 320 °C
800000 - 800000 cP

@Temperature 608 - 608 °F
Average value: 800000 cP Grade Count:1
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Viscosity 800000 - 800000 cP

@Shear Rate 25.0 - 25.0 1/s
800000 - 800000 cP

@Shear Rate 25.0 - 25.0 1/s
Average value: 800000 cP Grade Count:1
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..