Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 790000 cP @Temperature 25.0 °C |
790000 cP @Temperature 77.0 °F |
|
Esstech X-852-0000 FIT 852 Resin FIT 852 Resin is a novel low shrink urethane monomer based on Esstech's proprietary methacrylate technology. FIT possesses a volumetric shrinkage of 2.0 - 2.5% and conversion of 65 - 80% without fi.. |