Physical Properties Metric English Comments
Viscosity 78340 cP

@Shear Rate 5000 1/s,
Temperature 300 °C
78340 cP

@Shear Rate 5000 1/s,
Temperature 572 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers