Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 71 cP @Temperature 20.0 °C |
71 cP @Temperature 68.0 °F |
Absolute |
BASF Palatinol® 11P-E (DUP) Linear Phthalate Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing .. |