Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 50000 - 500000 cP @Shear Rate 1.00 1/s, Temperature 150 °C |
50000 - 500000 cP @Shear Rate 1.00 1/s, Temperature 302 °F |
Melt; Oscillating cone-plate |
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |