Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 50000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 50000 cP

@Temperature 25.0 °C
50000 cP

@Temperature 77.0 °F
at 2 rpm vibration
Permabond LH197 Anaerobic Gasketmaker
Permabond® LH197 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is highly flexible, making it ideal for dissimilar surfaces where differential th..
Viscosity 50000 - 500000 cP

@Shear Rate 1.00 1/s,
Temperature 150 °C
50000 - 500000 cP

@Shear Rate 1.00 1/s,
Temperature 302 °F
Melt; Oscillating cone-plate
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer
SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
Viscosity 50000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
50000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow DOWLEX™ 2507 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2507 Polyethylene resin is a narrow molecular weight distribution copolymer designed for fast injection molding of thin wall lids without warping. It has demonstrated excellent processabili..
Viscosity 50000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
50000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow DOWLEX™ IP-10262 High Density Polyethylene
DOWLEX® IP-10262 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution for use in reusable case applications including, poultry, fast food, a..
Viscosity 50000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
50000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow LDPE 993I Low Density Polyethylene
DOW LDPE 993I resin is a low slip, medium molecular weight distribution homopolymer designed to offer good gloss and rigidity with excellent flow characteristics. This resin has good processability ..
Viscosity 50000 cP

@Frequency 100 Hz,
Temperature 277 °C
50000 cP

@Frequency 100 Hz,
Temperature 531 °F
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..