Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 49290 cP @Shear Rate 5000 1/s, Temperature 285 °C |
49290 cP @Shear Rate 5000 1/s, Temperature 545 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |