Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 39000 - 480000 cP @Temperature 190 - 190 °C |
39000 - 480000 cP @Temperature 374 - 374 °F |
Average value: 164000 cP Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Viscosity | 39000 - 480000 cP @Shear Rate 300 - 5000 1/s |
39000 - 480000 cP @Shear Rate 300 - 5000 1/s |
Average value: 164000 cP Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |